Hi everyone!
I've done this formula before and it was a success, but this weekend I tried it out again and it was a complete failure even though I did everything as the last time, so I'm guessing it might be a temperature issue since I live in Sweden and it's winter here now. Anyway, if anyone here has tried formulating with SCI I would highly appreciate if you guys could help me troubleshoot this.
The formula is:
53% H2O
10& Cocamidopropyl betaine
10% Sodium cocoyl isethionate (with stearic acid)
5% Coco glucoside
10% Aloe vera juice
2% Glycerin
2% Hydrolyzed oat protein
2% Polyquaternium-7
2% Coco caprylate
2% Panthenol
0,5% Optiphen
1% Fragrance
1% Crothix
The issue here is that the SCI is mixed together with Cocamidopropyl betaine, I used a water bath and heated them and the rest of my water phase apart (exept for preservatives, fragrance, panthenol, polyquat and crothix). BUT the SCI simply won't melt.
I've read online that it has a melting point of 200 degrees celcius which is very high, I would say even for a regular stove so I'm guessing a water bath simply won't do. When I mix the 2 phases together the SCI simply forms a film floating on top and won't mix at all no matter how much I try to stir it in.
How do you guys use SCI, and how high do you usually heat it before it dissolves? I'm used to having water evaporate quickly even with a water bath so it scares me to just put it over a regular stove top.
Thank you so much!
I've done this formula before and it was a success, but this weekend I tried it out again and it was a complete failure even though I did everything as the last time, so I'm guessing it might be a temperature issue since I live in Sweden and it's winter here now. Anyway, if anyone here has tried formulating with SCI I would highly appreciate if you guys could help me troubleshoot this.
The formula is:
53% H2O
10& Cocamidopropyl betaine
10% Sodium cocoyl isethionate (with stearic acid)
5% Coco glucoside
10% Aloe vera juice
2% Glycerin
2% Hydrolyzed oat protein
2% Polyquaternium-7
2% Coco caprylate
2% Panthenol
0,5% Optiphen
1% Fragrance
1% Crothix
The issue here is that the SCI is mixed together with Cocamidopropyl betaine, I used a water bath and heated them and the rest of my water phase apart (exept for preservatives, fragrance, panthenol, polyquat and crothix). BUT the SCI simply won't melt.
I've read online that it has a melting point of 200 degrees celcius which is very high, I would say even for a regular stove so I'm guessing a water bath simply won't do. When I mix the 2 phases together the SCI simply forms a film floating on top and won't mix at all no matter how much I try to stir it in.
How do you guys use SCI, and how high do you usually heat it before it dissolves? I'm used to having water evaporate quickly even with a water bath so it scares me to just put it over a regular stove top.
Thank you so much!